This is my personal account: I take no responsibility for eating your cake.
(he/him)
After sitting in water for 2hrs then 10hrs, placed in a drying chamber at 70°C for 12hrs.
Print has retained the elasticity. The only notable change are some discoloration streaks from the stress of bending, but, these streaks also occurred prior to drying.
After sitting in water for 2hrs then 10hrs, placed in a drying chamber at 70°C for 12hrs.
Print has retained the elasticity. The only notable change are some discoloration streaks from the stress of bending, but, these streaks also occurred prior to drying.